Properties
Crystal optics, Nd:YAG Rods
1053 nm
within 3° of the crystal "a" axis
Nd
1% +- 0.2 % (by weight)
~ 480 +- 10 usec
~ 1.2 X 10~19 CM2
-
< 0.001 cm-1
25 dB
>=10J/cm2 for 1 ns laser pulse
1 ± 0.1 deg
< 10 arc sec
Better than lamba10 of wave at 632.8 nm
scratch dig 20-10 or better
@ 1053 inn with reflectivity per surface 5 0.25%
> 10J/cm2 for 10 ns pulses
Safety Information
Safety Information for this product is unavailable at this time.