Phone : +91-22-2207 0099
Email : info@ottokemi.com, sales@ottokemi.com


Specification Sheet

Monodispersed nanodiamond particles 10 mg/mL in NMP, carboxylated, 5 nm avg. part. size (DLS)

Detonation Nanodiamond, Nanodiamond

NDH 081

Detonation nanodiamonds find applications in polymer composites for providing improved mechanical properties, UV protection, and improved resistance to radiation.

Detonation nanodiamond (DN) was discovered in 1963, but for several reasons was known only among a small number of scientists until the turn of the century.

Properties

Nanotechnology products,Nanoparticle dispersions

Dispersion

10 mg/mL in NMP

+35.5 mV ± 20%

5 nm (DLS)


Safety Information

WGK Germany 1
Flash Point(F) 188.6 °F
Flash Point(C) 87 °C


PackingsPrice (INR)
5 ml 20007.00
5 x 5 ml POR

DisclaimerThe above particulars do not release the customer from the obligation to carry out an inspection of goods received.
Not for medical, household or any other uses, for lab use only, Please test before use.